by laser photonics | Aug 8, 2016 | Applications
Material: Titanium Method Used: Annealing Depth: Surface Laser Type: Pulsed Fiber Focal Length Lens: 160mm Power: 95% Frequency: 30 kHz Speed: 1″ per sec Passes: 12 Cycle Time: 26.52 seconds The samples were processed using the 20 watt Pulsed Fiber Laser...
by laser photonics | Aug 8, 2016 | Applications
Material: Foam Method Used: Cutting Depth: Kiss & (Through) Laser Type: CO2 Focal Length Lens: 3.75″ Power: 40 Watts (60 Watts) Frequency: 3 kHz (3 kHz) Modulated Speed: 300mm (300mm) Passes: 1 The samples were...
by laser photonics | Aug 8, 2016 | Applications
Material: Glass Method Used: laser marking Depth: Surface Laser Type: 100W CW CO2 (10.6um) Focal Length Lens: 300mm Power: 10% Frequency: 5kHz modulated Speed: 500mm/sec Passes: 5 Cycle Time:...
by laser photonics | Aug 8, 2016 | Applications
Application Details The Application was done with a low power system in the lab. The recommendation for this process would be for a minimum of 100watt laser for projected cutting speeds of 1mm per second. 100-watt laser projected 50mm plus per second.200-watt laser...
by laser photonics | Aug 8, 2016 | Applications
Material: Cardboard Method Used: Laser Cutting Depth: Through Laser Type: CO2 Focal Length Lens: 5″ Power: 200 Watts Frequency: 1-10 kHz (Modulated) Speed: 20-50mm Passes: 1 The samples were cut using the SBM 1200FL cutting system equipped with a 250 Watt...