695

Material:  Titanium Method Used:  Annealing Depth:  Surface Laser Type:  Pulsed Fiber Focal Length Lens:  160mm Power: 95% Frequency: 30 kHz Speed: 1″ per sec Passes: 12 Cycle Time: 26.52 seconds The samples were processed using the 20 watt Pulsed Fiber Laser...

689

Material: stainless steel   Power: 98%   Method Used: annealed   Frequency: 35 kHz   Depth: <.001   Speed: 5 inches per second   Laser Type: 20 Watt Q-Switch Fiber Laser   Passes: 1   Lens Focal Length: 160mm   Cycle...

683

Material:  aluminum Power:  50% Method Used:  etch Frequency:  35kHz Depth:  <.002 Speed:  25 inches per second Laser Type:  20 Watt Q-Switch Fiber Laser Passes: 1 Focal Length Lens:  160mm...